Keyes v. Pueblo Smelting & Refining Co.
Opinion of the Court
Two questions are made in the case by the defendants in opposition to the claim of the plaintiffs, and the first is that they deny that they have infringed the patent of the plaintiffs. The patent itself has relation to the art of smelting metallic ores, and is a very clear statement of a mode of withdrawing the pure metal after it has been separated by heat and the usual appliances of smelting furnaces from the other matter found in the ores in their native condition. And the mode by which this is done, as explained by the patentees, is a simple reliance upon some of the principles of natural physical science. They say, and that is undoubtedly true, that the metal — any metal which is sought to be extracted from these ores — is heavier than the other particles of ore, than the other matter found in the ore. The art of smelting, itself, consists in the processes by which, through the use of heat and other substances called “fluxes,” this mixture of the ore with calcareous matter, with some other metals, is separated, and the pure metal is in this manner disintegrated from, and in some shape brought to a separation from, the other more useless and less valuable parts of the ore. It is not necessary to inquire whether the ore of lead or of gold or silver or copper is merely a mechanical mixture,— as it mostly is, — or is in some cases a chemical mixture; the great result to be sought for in smelting is to separate them. • Lead is perhaps the easiest of all the ores to separate from the surrounding materials found connected with it. The mechanical principle to which I allude is that, these ores being mixed in a large furnace or cylinder without other materials which offer attraction to some of its elements, they are separated. It is by means of the heat secured through a blast-furnace. It is all melted, all dissolved, all turned into one fluid mass within the furnace, and precipitated from the upper part of the furnace, where they are mixed together, into the base of the furnace. In this process of separation and precipitation, or falling down, the metal being the heaviest,
“The products resulting from the smelting of lead ores, regardless of how the ores were previously treated, or what fluxes were added, are invariably— First, lead; second, matte; third, waste products. The mattels always tapped together with lead into a tap-hearth, in which the specifically lighter matte separates from the lead. It congeals much sooner than the lead, is taken off, and the lead is then ladled into moulds. The matte is never so poor as to be worthless. Generally matte is re-treated, and in a similar manner as the lead ores.”
Now, the usual mode of separating the “slag,” as it is called, which is the largest product of this smelting operation, and which is the lightest, is to make orifices in the cylinder or furnace, and that, being tapped in the liquid state, it flows off and is in various ways conducted away from the further operations of the smelter. The matte and the pure lead are then left, with an inclination in the pure lead to get to the bottom and the matte to the top; but this does not seem to be so readily separated, and so clearly marked, as the slag which runs off from the eye or holes in the furnace. The mode adopted by the plaintiffs in this case was to insert a tube precisely at the base of the furnace, which tube necessarily communicated with the pure lead alone; all the impurities, the matte and the slag, being at the top. The patentee of this invention does not seem to have concerned himself about what became of the slag nor of the matte, because, inserting his withdrawal tube at the base, the lower end •of the cylinder, he gets nothing but pure metal; and, as you will see by one of those plats there, or diagrams, his tube then bore an upward direction, and carried this pure lead to a bowl or basin. In this way, by the pressure of gravity in the furnace constantly forcing that lead out through the tube, and the slag and the matte not being able to mingle with it, but being used as a mere pressure with other lead that came down, working its way through, the pure lead was conveyed off, and separated from the matte and slag, and carried into the basin, from which it was ladled out, in the old-fashioned way, or perhaps carried out by another tube into moulds, and placed where they wanted it. But the thing to be done — the separation of the pure lead or any other metal from the impurities with which it was originally mingled in the ore— has been achieved, and the patent is for the mode of separating these materials, Of carrying away the pure silver from these other materials, •of smelting after it has been melted and after they have settled, the ore being still liquid, each having its place by virtue of gravity. That is his patent. He claims that he was the first man that ever did this in a way that did not require constant attention on the part of the smelter; that others made holes to let the metal run off, and then had to open .and watch them; that others run off the slag, and left the metal at the bottom, and, after the slag was all run off, that the matte and the metal
But the great defense relied on here is that the patent itself is not valid, because the principle on which it operates, and the description of the instrument itself, is to be found in the works of Mr. Karsten, a German, who had published a work on the subject of smelting and dealing with ores in Germany, where there are a great many mines, and where the science of mining has been, perhaps, as mqch considered as in any country in the world. I can hardly expect to enlighten anybody much on this subject. -It does not appear that Mr. Karsten ever made or invented a furnace for smelting. It is not known, as far as I know, whether he was a practical smelter. He seems to be a man of science, who undertook, by five volumes, to consider the science and the laws of smelting ores, and especially as they were understood in Germany. In his works he undertakes to describe the different kinds of furnaces. He mentions perhaps a dozen, and their modes of operation that were then in existence in Germany; and among others he describes a class of furnaces which are shown on that central diagram there, (Litharge furnace,) by which as the ore is melted it becomes fluid. The pure metal gravitates, as in other furnaces, to the bottom, and then is permitted to empty itself out into what he calls a “fore-hearth,” a little projection from the bottom of the furnace out into the open air, where the metal comes, and is dipped out by ladles, as it is in the one of the patentee’s. It is said that this is the same, or such a description of the mode of smelting as is to be found in the plaintiff’s patent. I have not been satisfied of that. In the first place, it is very clear from what is said here by Mr. Karsten himself, which I read, that the separation is not complete when it comes out into that fore-hearth or front. He declares that the matte, if not the slag, goes with it; that this matte, after it comes out, forms a covering over the pure metal, and before you can dip out that pure metal you
Case-law data current through December 31, 2025. Source: CourtListener bulk data.